Material: 99% alumina, sintered at a temperature of 1800°C for 40 hours.
Usage Instructions:
Do not contact with hydrofluoric acid.
Do not heat.
Never place in a drying oven.
After use, wash the mortar with water. If necessary, clean with dilute hydrochloric acid, then rinse thoroughly with water.
If stains remain, grind with a small amount of table salt for some time, then discard the salt and rinse again.
Al₂O₃ > 99%, excellent chemical corrosion resistance, good temperature resistance.
Formed by slip casting,
high density,
fine surface texture,
and strong wear resistance.
Product Specifications:
99% corundum mortar with 60mm rod
99% corundum mortar with 100mm rod
99% corundum mortar with 150mm rod
Reviews