Packaging: 100g/bottle, 400g/bottle.
Material name: dispersant.
Application: LFP/LFMP/carbon nanotube dispersion, etc.
Improving slurry fluidity and reducing slurry sedimentation can increase excellent properties such as the solid content of active substances.
Main Parameters:
| Item | Test method | Test results |
| Name | / | Dispersant |
| Appearance | Visual | Light yellow, waxy irregular large particles, |
| Composition | / | Block copolymer with conjugated groups |
| Solid content | Oven | 60±3 |
| Viscosity | Coating 4 cups | 5-25 |
| Density | Density cup | 1.02-1.03 g/ml |
| Recommended dosage | LFP/LMFP | 0.2-0.8% LFP/LMFP |
| Conductive carbon black | 20-60% conductive carbon black | |
| Carbon nanotubes | 20-60% carbon nanotubes | |
| Use and save | 1. The package is sealed and stored for 24 months. Keep it away from light, dry and sealed. 2. The material may clump, but it does not affect the performance. |
|