[BULK] NCM613 (polycrystalline) Nickel-cobalt-manganese Lithium battery ternary positive electrode material

Please consult customer service for prices

Nickel-cobalt-manganese NCM613 (polycrystalline) Lithium battery ternary cathode material polycrystalline ternary material.

XW-X

Note: This product category is Xiaowei’s bulk raw material supply, not a direct order product.

The price of this product is calculated by /KG or /m². You need to contact the customer service on the right to confirm the purchase needs before purchasing. Xiaowei will provide the most favorable price and shipping cost. Welcome to contact Xiaowei

The final price and technical parameters are subject to the Xiaowei customer service.

SKU: N/A Category:
To display brands list you need to create product attribute first. Go to Dashboard -> Products -> Attribute -> create new for your product brands. Then go to Theme Settings -> Shop -> Brands and set the newly created attribute. Be sure that you have added some brands to that attribute also.

Xiaowei New Energy provides NCM battery materials in bulk, 2KG-100KG.

Lithium ion battery cathode electrode, Ni, Co, Mn NCM material, morphology as secondary sphere, excellent rate performance

Main Parameters:

Test item Unit Specifications Actual
measurement
results
Testing
methods or
instruments
Chemical
composition
Li (wt%) 7.0±2.0 7.52 ICP
Co+Ni+Mn (wt%) 60.0±3.0 58.88
Ca (wt%) ≤0.01 0.0015
Cu (wt%) ≤0.001 0.0000
Fe (wt%) ≤0.01 0.0014
Mg (wt%) ≤0.01 0.0015
Na (wt%) ≤0.01 0.0095
Free lithium (wt%) ≤0.5 0.0774 Acid
burette
Physical
characteristics
Particle
size
distribution
D10 (μm) ≥1.0 2.33 Laser
particle size
analyzer
D50 (μm) 4.0~6.0 5.06
D90 (μm) ≤15.0 10.88
BET (m2/g) ≥0.5 0.78 Fully
automatic
surface
area and
porosity
analyzer
TD (g/cm3) ≤2.5 1.95 Vibrating
density
measuring
instrument
Moisture (ppm) ≤2500 166.3 Moisture
meter

Packaging requirements: Vacuum packaging with aluminum-plastic film, outer layer packaged in plastic bags.

Storage requirements: Sealed, stored in a cool and dry place.

The material needs to be vacuum sealed for storage

The material is prone to water absorption, and humidity control is required throughout the entire production process

The electrolyte used during testing is NCM electrolyte

Baking conditions for electrode: Bake at 85 ℃ for 4 hours

 

 

Weight N/A

Reviews

There are no reviews yet.

Be the first to review “[BULK] NCM613 (polycrystalline) Nickel-cobalt-manganese Lithium battery ternary positive electrode material”

Your email address will not be published. Required fields are marked *

You have to be logged in to be able to add photos to your review.

This part of the content is being sorted out by Xiaowei
Shopping cart
Sign in

No account yet?

Create an Account

Get a Fast & Accurate Quote

Our sales engineers will provide a customized quotation and technical support within 24 hours.